Product Range:
Section/Profiles: AS PER CUSTOMERS REQUIREMENT.
- Self lubricant graphite bushes
- Aluminum bronze
- Leaded bronze
- Gunmetal
- Tungsten Copper
- Cadmium Copper
- Chromium Copper
- Beryllium Copper
- Sulphur Copper
- Tellurium Copper
Description
Chemical Properties for Rods/Bushes/Sections | ||||||||||||
ALLOYS | Cu % | Zn % | Ni % | Sn % | P % | Si % | Mn % | AS % | PB % | FE % | AL % | OTHERS % |
AL.BZ. CA 103 | REM | 0.4 | – | – | – | – | 0.5 | – | – | NL+FE 4.0 | 8.8-10 | 0.5 |
AL.BZ. CA 104 | REM | 0.4 | 4.0-6.0 | 0.1 | – | – | 0.5 | – | 0.05 | 4.0-6.0 | 9.0-11 | 0.5 |
Chemical Properties for Special Alloy Rods/Bushes/Sections | |||||||
ALLOYS | COPPER % | TELLURIUM % | SULPHUR % | CADMIUM % | CHROMIUM % | BERYLLIUM % | OTHERS |
TELLURIUM | 99.8 MIN+AG | 0.3-0.7 | – | – | – | – | 0.03 MAX |
SULPHUR | 99.8 MIN+AG | – | 0.3-0.7 | – | – | – | 0.03 MAX |
CADMIUM | REM | – | – | 0.7-1.2 | – | – | 0.02 MAX |
CHROMIUM | REM | – | – | – | 0.6-1.2 | – | 0.03 MAX |
BERYLLIUM | 99.8 MIN+AG | – | – | – | – | 1.6-1.8+COBALT 0.2-0.4 | – |
Class | Chemical Composition (% by wt.) | Density | Conductivity | Resistivity | Hardness | Bend Strength |
Copper max. additves tunsten | gr/cc | Min. IACS % Min. | μΩ*cm Max. | HB Kgf/mm2 | Min. MPa Min. | |
W50/Cu50 | 50 ± 2.0 0.5 balance | 11.85 | 54 | 3.20 | 115 | …. |
W55/Cu45 – | 45 ± 2.0 0.5 balance | 12.3 | 49 | 3.50 | 125 | …. |
W60/Cu40 | 40 ± 2.0 0.5 balance | 12.75 | 47 | 3.70 | 140 | …. |
W65/Cu35 | 35 ± 2.0 0.5 balance | 13.3 | 44 | 3.90 | 155 | …. |
W70/Cu30 | 30 ± 2.0 0.5 balance | 13.8 | 42 | 4.10 | 175 | 667 |
W75/Cu25 | 25 ± 2.0 0.5 balance | 14.5 | 38 | 4.50 | 195 | 706 |
W80/Cu20 | 20 ± 2.0 0.5 balance | 15.15 | 34 | 5.00 | 220 | 736 |
W85/Cu15 | 15 ± 2.0 0.5 balance | 15.9 | 30 | 5.70 | 240 | 765 |
W90/Cu10 | 10 ± 2.0 0.5 balance | 16.75 | 27 | 6.50 | 260 | 804 |